产品特性:
发泡底/通透PVC地板专用胶
超大涂布量
良好的耐水性
优异的粘结力
水性环保
施工方法:
使用前应充分搅拌均匀。建议用A1、A2锯齿刮刀均匀的涂刮,铺展后晾胶时间在5-30分钟,即可铺设上述地面材料。
注意事项:
铺下地板后先用软木板推压,再用30KG以上的辊筒滚压以排除残余的空气,确保粘合剂全部粘合到地板的背面。要确保良好的通风和对施工最佳的温度和温度条件。低温或高温度会明显地延长干燥时间或推迟粘结强度的发展。在粘结剂的强度还未完全达到前,要防止过度使用。
Features:
Foaming
Base Coat / Special Adhesive for Penetrating PVC Floor
Super
Coating Weight
Excellent
Waterproof Performance
Excellent
Bonding Strength
waterborne
environmental protective
Construction
Method:
Stir
it evenly before usage. It is suggested to use A1 or A2 sawtooth blade and lay
the ground for 5 to 30 minutes before laying the materials above.
Notices:
Press the new laid floor by soft wood panel then
a roller (more than 30kg) to remove the redundant air to ensure the adhesion
between the bonding agent and the floor. Ensuer the good ventilation,
temperature and humidity for construction. Lower or higher temperature may
delay the time for drying or influence the bonding strength. Don't over use it
before the bonding strength is not reached. S